7. Simulate ordered crack growth¶
The plate crack tutorial follows a through crack and a surface crack from their initial profiles to their final dimensions, using a NASGRO material fit and the same tensile load history for both cases.
Open lesson 33 to compare
both plate geometries using the same ordered load blocks. The plots align
applied stress, crack dimensions, and peak stress intensity on cumulative
cycles. To edit and rerun it locally, use
uv run marimo edit notebooks/33-ordered_crack_growth.py.
Open lesson 34 to generate a long tensile waveform and follow it to a Miner damage limit and a crack-growth toughness stop.
Use the family notebooks to run ordered crack propagation and overlay the initial and last accepted profiles. Through cracks · lesson 35 · Surface cracks · lesson 36
For an SC07 circular surface crack in a round bar, open lesson 36 or follow the same three tensile load blocks through MCP.
Choose a geometry and tensile load¶
Match the crack shape and loading direction to a supported case. Check the dimensions and validity limits in the geometry reference. Supply the tensile load blocks in their original order.
Material inputs¶
Use a calibrated NASGRO curve with parameters in MPa, mm, and MPa·√mm. See the material parameter reference.
Solver controls and result¶
The following center-cracked plate example uses two tensile load blocks and a synthetic NASGRO curve.
from py_fatigue.crack_growth import (
CenterThroughCrack,
LoadBlock,
NasgroCurve,
simulate_crack_growth,
)
geometry = CenterThroughCrack(half_width=50, half_length=5)
curve = NasgroCurve(
coefficient=1e-10, exponent=2, p=0.5, q=1,
threshold_zero=25, threshold_fanning=0, toughness=500,
constraint=2, peak_to_flow=0.3,
)
loads = [LoadBlock(0, 40, 8.5), LoadBlock(10, 50, 10)]
result = simulate_crack_growth(
geometry, curve, loads,
max_cycle_step=1, length_tolerance=1e-6,
cycle_tolerance=1e-4, max_trials=40,
)
print(result.termination, result.final_cycles)
Expect spectrum_exhausted at 18.5 cycles. Compare the last accepted
geometry with the initial flaw. The
solver reference
describes the controls, output conventions, and validation cases.
Plot the geometry, material law and result¶
Call geometry.plot() or geometry.echarts() to draw the initial plate
crack. Pass result=result to overlay the last accepted profile.
Surface cracks are drawn in the crack plane of the plate, pipe, bar, or
thread. If a run stops before accepting a state, the plot shows the
starting geometry.
fig, ax = geometry.plot(result=result)
geometry.echarts(result=result)
Call curve.plot() or curve.echarts() to show the long-crack reference
curve at stress ratio R = 0 (k_min = 0). Both sweep maximum stress
intensity up to toughness and mark that limit with a dashed line. Supply
length to apply the finite-crack correction to the growth threshold and
k_min to change the minimum stress intensity.
fig, ax = curve.plot()
curve.echarts()
fig, ax = curve.plot(length=4.0, k_min=20.0, scale="loglog")
fig, ax = result.plot()
result.echarts()
A scalar k_max sets a shorter sweep endpoint. Supply an array to evaluate
exact sample points, or a one-element array to show one point. With explicit
samples, k_min can be one value or an array paired with k_max.
Use scale="semilogx" to show zero growth below threshold, or
scale="semilogy" for the default logarithmic growth-rate axis.
To compare results on shared axes, use other_result.plot(ax=ax,
label="Surface crack"). The plot uses the accepted points in
result.history.